Electronics Forum | Wed Aug 31 04:04:32 EDT 2005 | Slaine
im running some tests at the moment for hand soldering using a no residue water based flux from MBO, called WBF-01. leaves a good clean finish.
Electronics Forum | Mon Oct 03 14:22:23 EDT 2005 | davef
You'll still have to dispose of filters and whatnot and recycle your water polishing system tanks as hazardous materials.
Electronics Forum | Wed Aug 27 13:11:19 EDT 2008 | dwelch123
We roll ours up, fingers and all, and soak them for about an hour in a solution of water and DOMINATE (heavy duty degreaser) you can order from Grainger. They come out looking brand new every time!
Electronics Forum | Thu Nov 21 12:06:16 EST 2013 | rgduval
The last time I got corroded parts out of my wash was when my DI tanks were spent, and I was pretty much using straight tap water. Refreshing the DI tanks eliminated my issue. Hope this helps. cheers, ..rob
Electronics Forum | Thu Dec 03 15:41:09 EST 2015 | proceng1
We do run them through an Aqueous washer, but I don't see excessive deposits or anything before washing. And our wash is just heated DI water.
Electronics Forum | Wed Jul 24 10:07:44 EDT 2019 | ameenullakhan
Hi Team, Can anyone suggest me best stencil opening for CCGA. Attached is the component details. Solder paste : water solube - ORL0 - Jtsd 001 ( Sn63/Pb37) Any one has qualified the same. Regards, Ameen
Electronics Forum | Wed May 20 16:07:22 EDT 2020 | stephendo
You want a big enough storage tank to smooth pressure. Figure out what size pipes you need and go a size bigger. Make a loop of the pipes with shut offs. That way you can shut down any section and still have air to the rest of the air line. Run the p
Electronics Forum | Mon Dec 02 16:01:15 EST 2002 | russ
If you can, attach athermocouple to the locations where you are getting solder balls. A previous product I had showed the same thing and we found that we had inadequate preheat leaving the liquid flux to splatter when it hit the wave. It could aslo
Electronics Forum | Mon Dec 02 17:02:28 EST 2002 | Vince Whipple
Steve, I agree with the recommendation to check the temperature. This is the first place to go. Is this an IPA or water based Noclean? What is the topside temp of the assembly at the effected areas? If you are too cold you will have a tendency to hav
Electronics Forum | Thu Dec 03 15:30:00 EST 2015 | ttheis
We've started off with Kester 951 'no-clean' so far which is alcohol based I believe. It seems to do very well with foaming, activation and low residue, but if we can move to water based and get good results that would be great. The 951 flux and thin