Electronics Forum | Thu Apr 01 21:18:31 EST 1999 | Chris Kelly
Glenn, There are both very good VOC-Free fluxes as well as alcohol based fluxes out there. This should be your primary focus if you are so lucky as to have to opportunity to actually select a flux! The use of nitrogen will benefit any no-clean pro
Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon
| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a
Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon
| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered
Electronics Forum | Sun May 23 07:13:56 EDT 1999 | Scott Cook
| Has anyone had any experience or data using vibration during the reflow process. | We introduced a vibration device attached to the fixed rail on a Vitronics reflow oven. The reason was to prevent skewing on large PLCC devices. The process worked v
Electronics Forum | Wed Jan 11 22:47:31 EST 2006 | davef
We didn't intend to light anyone's fur on fire [get anyone's underwear in a knot, roil the waters, have a cow man] about consultants. The Phil Zarrow wrote a useful paper that could help in evaluating paste. Here read it ... Evaluating Solder Paste
Electronics Forum | Thu May 26 08:52:42 EDT 2011 | davef
Phil Zarrow wrote a useful paper that could help in evaluating paste. Here read it ... Evaluating Solder Paste � Not An Option Contributed by Phil Zarrow of ITM an Independent SMT consulting firm With soldering being the dominant source of assembly