Electronics Forum | Tue Dec 20 10:10:21 EST 2005 | SteveH
Ours is the same configuration as that, we run with neat Humiseal 1B31 through the needle valve and a 1:1 blend 1B31/Butanone (MEK) in the spray valves. Programming is done via a PC using the pendant and the path is point to point trained on scrap P
Electronics Forum | Thu Jun 05 18:11:53 EDT 2008 | jlawson
Also coating costs depends on solids content vs final dry film thickness. Some newer UV coatings are 100% solids, so what you put down you get on the PCB after cure, use no solvents at all. So a cost to look at are qty of PCB per litre of material. T
Electronics Forum | Fri Jan 25 14:30:56 EST 2002 | stimpman
All, On my Wave Machine the Coating on the fingers "pcb carriers" is coming off. They are way way way way overpriced to replace if all possible. I would think there is someone out there that could re-coat them??? If so what is the companies name/ c
Electronics Forum | Fri Feb 11 16:34:01 EST 2000 | Chris McDonald
Does anybody have a source for jigs/tanks for a manual dip operation? We are stuck conformally coating PCBs manualy and the volumes do not justify us buying a 100k automated machine. there for we have to manually dip the pcb in a silicon based coatin
Electronics Forum | Thu Sep 09 10:50:59 EDT 2004 | agkettle
Does anyone have any experience with underfill of HD connectors? New customer wishes to underfill 6 HD connectors that have been pressed into PCB. Capillary action is causing the conformal coat to wick up into connector. Material is acrylic.
Electronics Forum | Tue Oct 06 15:50:12 EDT 1998 | Bill Tuttle
We are experiencing poor wetting on various components placed on a PCB with En-Tek coating. Is anyone else experiencing simular problems ? We have the following questions: 1. How can the thickness of the En-tek coating be measured? 2. Is En-tek vol
Electronics Forum | Wed Aug 04 14:34:50 EDT 1999 | Dave F
| Has anyone out there tried to parylene coat plastic parts prior to soldering them to a pcb? I'm looking at several potential applications where fewer than 5% of my components on a pcb are plastic, yet from a reliability aspect (environmental condit
Electronics Forum | Thu May 02 14:07:53 EDT 2013 | duso02
I would suggest lowering the viscosity even more. Humiseal even sells 1B31 pre-mixed specifically for spray machines and the highest they go is 65cps.
Electronics Forum | Thu May 02 14:26:57 EDT 2013 | wahahasteven
Thanks for the advise, but we want to change the lacquer/thinner ratio at the last step if we don't have other solution.
Electronics Forum | Mon Jun 18 14:35:40 EDT 2018 | davef
That's a reasonable question for a supplier to ask his / her customer. It depends ... It depends on the materials use in the process the assembly and the reflow temperature recipe
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830