Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2719
What risk I have if I left solder balls on some pcb?
...
- Mar 30, 2009
by
Armando_Gomez
depending on what is diameter of your balls ;)
and smallest...
- Mar 31, 2009
by
d0min0
Solder ball formation can be a significant problem if the ba...
- Mar 31, 2009
by
davef
lol!, they are in the middle of some 0805 and the diameter d...
- Mar 31, 2009
by
Armando_Gomez
What you have described are actually called Solder Beads for...
- Apr 03, 2009
by
EMS-Engineer
Thanks I will read it
:o)
...
- Apr 04, 2009
by
Armando_Gomez