hello, I have been experiencing a strange solder defect late...
- Sep 20, 2019
by
bukas
Looks like poor wetting/solderability to me. I don’t see hee...
- Sep 20, 2019
by
DeanM
Yes, no wetting on the several leads, to verify is same loca...
- Sep 22, 2019
by
sssamw