Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Is any one else having a problem with parts that are Ni/Sn p... - Jun 14, 2004 by Jsmith
How old are these parts? Sn/Ni plating is very succeptable ... - Jun 14, 2004 by RDR
The parts are dated Mar 20 2004. My profile hits a peek of ... - Jun 15, 2004 by Jsmith
Well take away the easy answers! How are the parts falling ... - Jun 15, 2004 by RDR
It seems like the break is happening between the sn and ni. ... - Jun 15, 2004 by Jsmith
have you tried a more agressive flux like water soluble to s... - Jun 16, 2004 by RDR
I ran some test samples with a water soluble past (Amatech w... - Jun 16, 2004 by Jsmith
Well I am clueless! I have a lead free build coming up and ... - Jun 16, 2004 by RDR
It sounds like the parts are not soldering properly [have po... - Jun 17, 2004 by davef