Good morning, Once again a met annoying solder beading is... - Mar 18, 2006 by Hypnotia
hi same sort of broblem v r getting after reflow. i am no... - Mar 19, 2006 by ausajid
Good morning, In this case separation speed doesn�t affec... - Mar 20, 2006 by Hypnotia
Pavel Point: You suspect that solder paste can easily get... - Mar 20, 2006 by davef
Good morning Dave, Here are some of my assumptions. Pleas... - Mar 21, 2006 by Hypnotia
If you usually get good release on other products with your ... - Mar 21, 2006 by jdengler
Ahoj Pavele, di you considered to try a Type-3 solder pas... - Mar 21, 2006 by
1 Chatter about mask opening � No BIG problems with these st... - Mar 21, 2006 by davef
Good afternoon, We can use type-3 solder paste, but what ... - Mar 23, 2006 by Hypnotia
Check placement pressure. I agree with the "smushing" theory... - Mar 23, 2006 by