Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Solder Paste

Views: 2001

manyhatz

#40739

Solder Paste | 30 March, 2006

Does anyone have experience with Multicore WS200? is it any good?

reply »

#47727

Solder Paste | 16 February, 2007

I have been using the Loctite Multicore WS200 with great results for the last two years. We also use the lead free version WS300. I like the flux chemistry (which is the same for both products); it really withstands long soaking times and with very good wetting results. We process dense thick PCB Immersion Silver finish.

Does anybody have had a bad experience with Multicore products? Any cons or issues identified on any of these two products?

reply »

best reflow oven

Small Parts Tips