Component Terminals with silver plating | 20 April, 2006

hi All, recently i have received some parts with the lead turning black, and i then found out the leads are silver plating, is that going to be a problem? or it is simply a cosmetic issue? pls advise ASAP!! thansk a lot!!

reply »

GS

#41101

Component Terminals with silver plating | 20 April, 2006

Silver tarnish on lead could compromise the soldering, mainly in case of No Clean process. Make sure components are correctly packaged and stored. Check the vintage ( Manufacturing Data Code) and in order to avoid them to get old on shelf make sure FI-FO procedure is in place. etc.

Regards......GS

This message was posted via the Electronics Forum @

reply »

#41219

Component Terminals with silver plating | 26 April, 2006

weve hand soldered a few components that were tarnished with no problems, also the tarnish is electrically conductive if it helps.