Reflow oven | 24 April, 2006

Hello guys,

I am Looking for a oven with the following specifications.

Can any one suggest me the best suitable model. Thanks ========================================================== - heating length 2500mm - zone top/bottom 7 - forced convection - start up time ~ 40min. - Lead free and nitorogen compatibility - Min. Process temp. 300degree C - Delta T +/- 1.5 Degree C - Chain Conveyor - Speed 0.2 to 1.8 m/min. - conveyor width 50/450 ( min/ max ) - clearance top/bottom 70mm/45mm - Infeed / outfed lenght 300 / 200mm - Cooling zone length 300 - Cooling system in unloading area 400mm min. - Noise level less than 70 db - CE/JIS/Equiqvalent certificate

reply »

#41151

Reflow oven | 24 April, 2006

Hello TA,

Novastar's Model 18X2HT sounds like it will meet most of your requirements. If you would like detailed information about it, please contact me at pjshiloh@novastarinc.com. or (215)947-4700.

Regards, John Shiloh