Hi all guys what impact does red eye on the epcb have when the solder mask is not uniform to the layer. I am having trouble with quality.

reply »

#42756

RED EYE | 17 July, 2006

We're not familiar with "red eye".

reply »

#42782

RED EYE | 18 July, 2006

FWIW, neither are we, at least in this context.

reply »

Chunks

#42784

RED EYE | 18 July, 2006

It's generally followed by the munchies.

"Don't forget a towel!"

reply »


RDR

#42802

RED EYE | 19 July, 2006

I have no idea whats going here

Russ

reply »

Cartman

#42804

RED EYE | 19 July, 2006

#42805

RED EYE | 19 July, 2006

I think I may get in trouble if I goto websites that contain the words "poopshoot". I can see myself explaining that one to HR.......

Oh mey !

reply »

Chunks

#42806

RED EYE | 19 July, 2006

I do believe Russ knows exactly what's going on, or should he say it Towelie voice "I have no idea what's going on..."

Now I have to go play Funky Town on the keyboard of my placement machine.

reply »


RDR

#42807

RED EYE | 19 July, 2006

hehehehee Got me pegged Mr chunks!

reply »

Chunks

#42822

RED EYE | 20 July, 2006

Mr?

reply »


Rob

#42832

RED EYE | 20 July, 2006

What you get up to at weekends is totally fine with us! Perhaps you've been working out too hard????

reply »

Reflow Oven

Fluid Dispense Pump Integration