when I order a thermocouple wire for doing oven profiles, it...
- Jul 20, 2006
by
fordf1502004
based on experience, no significant change.
...
- Jul 21, 2006
by
Reypal
How do you plan on fusing the wires back together ?
...
- Jul 21, 2006
by
Sr. Tech
Cut the loose ends and not the couple?
Russ
...
- Jul 21, 2006
by
RDR
The ones we use are sealed on the plug end.
...
- Jul 21, 2006
by
Sr. Tech
you can use a thermocouple welder to fuse the wires back. as...
- Jul 21, 2006
by
Amol Kane
Not to argue, but you can use a spot welder to fuse thermoco...
- Jul 21, 2006
by
davef
Addressing the issue "Will cutting change the readings?" Ver...
- Jul 24, 2006
by
nodlac