thermocouple wire | 20 July, 2006

when I order a thermocouple wire for doing oven profiles, it comes in a standard length of 36 inches, will there be any effects if I were to cut the wire down to 9 inches? Will cutting change the readings?

reply »

#42853

thermocouple wire | 21 July, 2006

based on experience, no significant change.

reply »

#42866

thermocouple wire | 21 July, 2006

How do you plan on fusing the wires back together ?

reply »


RDR

#42874

thermocouple wire | 21 July, 2006

Cut the loose ends and not the couple?

Russ

reply »

#42882

thermocouple wire | 21 July, 2006

The ones we use are sealed on the plug end.

reply »

#42884

thermocouple wire | 21 July, 2006

you can use a thermocouple welder to fuse the wires back. as a matter of fact we use the welder to create thermocouple junctions. this is way less expensive that buying already formed thermocouple junctions.

reply »

#42886

thermocouple wire | 21 July, 2006

Not to argue, but you can use a spot welder to fuse thermocouple wires, also.

reply »

#42913

thermocouple wire | 24 July, 2006

Addressing the issue "Will cutting change the readings?" Very Very Doubtful.

Here is a link to a helpful guide.

http://www.omega.com/techref/