CAF

Views: 3449

GS

#42928

CAF | 25 July, 2006

Hello all,

I need to learn about Conductive Anodic Filament (CAF).

All information about the phenomenon will be appreciated.

About IPC TM-650 6-2-25 CAF Resistance Test, where could it be performed in European Lab ?

Thanks in advance

Regards.....GS

This message was posted via the Electronics Forum @

reply »

#42945

CAF | 26 July, 2006

Burn again to you Chunks ala Davef!!!

reply »

mumtaz

#42953

CAF | 26 July, 2006

Hi Doc!

Yeah, high fives all around. You guys are awsome.....

reply »

#42991

CAF | 27 July, 2006

Do not slander my name you devil!

reply »


Rob

#42997

CAF | 27 July, 2006

Yeah, I agree with you for once Doc.

It's quite obvious you don't need any help on that front you're doing a perfectly good job all on your own.

reply »

#43000

CAF | 27 July, 2006

Thank you sir.

reply »

GS

#43109

CAF | 1 August, 2006

Thank you so much Gents

Best Regards..............GS

This message was posted via the Electronics Forum @

reply »

GS

#43817

CAF | 7 September, 2006

If I am not wrong, by reading so huge amountof infos, it seams that CAF test is justified (suggested) if the PCB has at least 4 layers. Correct?

What about in case of a need to perform a CAF test ona 2 layers PCB ?

Thank you

Best reagrd.....GS

reply »

#43853

CAF | 11 September, 2006

We expect that CAF can form on a 2-layer as easily as a 4 layer board.