finger print

Views: 1616

new guy

#46471

finger print | 3 January, 2007

I'm a new guy in this field. I have a question about solder paste process. Is there any effect to the solderbility if we do a lot of contact to copper pad without using any insulation ( direct to the finger ). Where can i get information about smt process? Any recommended website @ paper?

reply »


RDR

#46489

finger print | 4 January, 2007

do not touch copper boards, use cotton gloves.

IPC 610 has some handling guidelines that you may want to look at.

Russ