SAC 305 Reflow & SN100C Wave and Selective

Views: 2498

#47661

SAC 305 Reflow & SN100C Wave and Selective | 15 February, 2007

Is there anybody out there doing this scenario:

SAC 305 Reflow & SN100C Wave and Selective

Can the 2 alloys be mixed on 1 board, say, SAC 305 for SMT, and SN100C for thru-hole? Are 2 different rework chemistries needed, or can one use SN100c wire or SAC 305 wire and touch up either type of joint?

Thanks in advanced.

reply »


RDR

#47673

SAC 305 Reflow & SN100C Wave and Selective | 15 February, 2007

They are all compatible with each other. Data is at alpha metals website and FCT assembly

Russ

reply »

Cmiller

#47675

SAC 305 Reflow & SN100C Wave and Selective | 15 February, 2007

Russ is correct. We have been using SAC 305 for SMT and SN100C for wave and selective and repair for about a year. May switch to SN100C in SMT at some point if we can get some paste that wets better.

reply »

#47848

SAC 305 Reflow & SN100C Wave and Selective | 20 February, 2007

We have been using SAC 305 for reflow and Cobalt 995 (very similar to SN100C, only cheaper) for wave and rework for quite a while now with no issues that I'm aware of.