Is anyone doing this? What is the proper temp to bake tubes ...
- Mar 01, 2007
by
jdumont
JDumont,
Baking in tubes is possible. Max temp for tubes ...
- Mar 05, 2007
by
Well that is completly unacceptable for me and im sure 99% o...
- Mar 05, 2007
by
jdumont
We've got away with 90C before, however at 120C they tend to...
- Mar 05, 2007
by
Rob
Yea, we have A LOT of tubes. We use lots of SOICs. I need to...
- Mar 05, 2007
by
jdumont
Join the "big issue" club.
We were just reading the "fine...
- Mar 05, 2007
by
muse
Nitrogen cabinets.
...
- Mar 05, 2007
by
I've wondered about the 5% spec myself. Section 4.2 points ...
- Mar 05, 2007
by
Bman
De-Humidification cabinets. The draw back with Nitrogen is t...
- Mar 05, 2007
by
paul_stamper
Baking, IC tubes, metal
* Perfection Products; 1320 S Indi...
- Mar 05, 2007
by
davef
Table 4-1 only specs the humidity requirement for bake tempe...
- Mar 06, 2007
by
muse
Let me explain. At 125 degrees C, the oven is above the boil...
- Mar 25, 2007
by
Stu Leech
That's what I thought. The humidity req't would be a non-is...
- Mar 26, 2007
by
muse
The issue is of drying moisture-sensitive surface-mounted pa...
- Mar 26, 2007
by
Stu Leech
Paul:
You are dead-on! Desiccant and nitrogen cabinets ar...
- Mar 26, 2007
by
Stu Leech