Hello,
We are having issue with one of the customer boar...
- Mar 05, 2007
by
On your ENIG thickness requirements, search the fine SMTnet ...
- Mar 05, 2007
by
davef
Hi Mark,
Solder paste will not flow on Ni like it appears...
- Mar 06, 2007
by
Real Chunks
Hello,
We replated the boards with new Ni and Au and the...
- Mar 07, 2007
by
Well there ya go, this proves you can't engineer from your d...
- Mar 07, 2007
by
Real Chunks
ENig can vary in quality, but I've never seen an ENiG board ...
- Mar 08, 2007
by
Dirk Nuendyke
There is nothing to argue if you had found Ni above or togat...
- Mar 11, 2007
by
Mark