Dear Friend,
I appreciate some one can give some opinion re...
- Apr 11, 2007
by
ray
On one hand, nothing in 8.2.5.4 that states that you need a ...
- Apr 12, 2007
by
davef
If the solder joint meeting 8.2.5.4, minimum side joint leng...
- Apr 12, 2007
by
ray
We'd say yes, if it meets both 8.2.5.4 and 8.2.5.6
...
- Apr 12, 2007
by
davef
Davef,
Thanks for your reply. Also sorry because I didint n...
- Apr 13, 2007
by
ray
Your paste should meet the mid-point of outside lead bend. I...
- Apr 13, 2007
by
davef