Hi All, Via X-rays, we found solder voids appear on PTH l... - Aug 18, 2007 by Sean
What are you trying to do: * Improve hole fill? * Reduce P... - Aug 19, 2007 by davef
Do you of reducing hole size of DIMM connector will improve ... - Feb 19, 2008 by dd
Duno. What's the diameter of: * Finished connector lead * ... - Feb 19, 2008 by davef
Connector pin - 10.83 mils Hole dia - 27 - 33 mils. We are... - Feb 19, 2008 by dd
We'd go with the formula above. ... - Feb 20, 2008 by davef
We had a similar problem with lead-free through-hole compone... - Feb 20, 2008 by Tony SMT
ni, I had similar problem too.I bake PCB in SW mashine - ... - Feb 20, 2008 by iv40
iv40, I don't suppose you know/remember what base material y... - Feb 20, 2008 by Tony SMT
hi,Toni, we use only FR4.Some of PCB we order in China an... - Feb 21, 2008 by iv40
We have prob Solder voids for Connector, Micro D. We used HM... - May 06, 2009 by radzi