Hi,

we use om338 from alpha metals in our smt production lines.I wont change this solder paste with kester em 918.Is anybody use this solder paste?what yo think abaout this paste.Is it good?

reply »


aj

#51629

kester em918 | 2 September, 2007

Hi,

I also use OM338 and would be very reluctant to use any other product. I have trialled 3 or 4 other top brands but cant find anything that ticks all the boxes.

aj...