IPC standards for TR-640A

Views: 2192

#51813

IPC standards for TR-640A | 17 September, 2007

Is anybody using IPC TR-640A? This is a troubleshooting checklist for wave soldering. Is it worth looking at?

reply »

#51814

IPC standards for TR-640A | 17 September, 2007

We have TR-460A. We do not use it very often, because of the level of experience of our troop. It is useful for companies looking to develop, structure, and organize their wave soldering process troubleshooting skills. The information in TR-460A is not particularly novel. It presents things that are available other places, but if you don't have those other resources, it could be a worthwhile purchase.

reply »