Q1: Can Stainless steel be soldered?
A1: Yes, stainless ste...
- Jan 03, 2008
by
davef
Davef, thnx for your reply. Sorry, forgot to clarify "our no...
- Jan 03, 2008
by
fsw
Patrick, thnx for your info. The tabs will be soldered on a ...
- Jan 03, 2008
by
fsw
Stainless steel can NOT be soldered with the solder that is ...
- Jan 03, 2008
by
Dirk Nuendyke
Recommended procedure for soldering stainless steel [Atlas S...
- Jan 03, 2008
by
davef
Consider conductive epoxy. Among the suppliers that make the...
- Jan 03, 2008
by
davef
Why are you using stainless steel? Corrosion resistance? Ca...
- Jan 03, 2008
by
Flipit
So, I'd have to grind the living sh#t out of my wedding ring...
- Jan 04, 2008
by
Dirk Nuendyke
All,
The reason SS (stainless steel) was being considered...
- Jan 04, 2008
by
fsw
Good move. Again, stainless can NOT be soldered with standa...
- Jan 04, 2008
by
Dirk Nuendyke
they make tin plated steel batt contacts. may be your best o...
- Jan 07, 2008
by
RDR
Another thing I'm curious about. What is the "functional pu...
- Jan 07, 2008
by
Dirk Nuendyke
All must be cautioned when messing with acids. Of course, ne...
- Jan 07, 2008
by
mparker
might try solder-less through hole connector technology for ...
- Jan 07, 2008
by
mparker
If your wedding ring ever gets hot enough to melt solder, I ...
- Jan 08, 2008
by
jmelson