Qualitek Super Deox H

Views: 2760


GSx

#53232

Qualitek Super Deox H | 16 January, 2008

Hello,

does anyone of you have experience by using Qualitek Super Deox H, dross reducer on Lead Free solder pot ?

Any concern by using it ?

Thank you

Regards......GSx

reply »

#53236

Qualitek Super Deox H | 16 January, 2008

A couple years ago there was a buzz here on SMTnet about P. Kay Metal MS2. The Super Deox sounds smilar.

reply »

#53257

Qualitek Super Deox H | 18 January, 2008

KRIKIES! As the Scottish say, "The best-laid schemes of mice and men often go astray."

P.K. Metal's star has faded for some strange reason. Is P.K. Metal's product the "Vioxx" of the wave deoxidizing industry?

Rumour has it it turns your wave solder into a swamp.

reply »