Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Able To Post Image

Views: 7627

#53319

Able To Post Image | 22 January, 2008

This is a picture of hypercorroded nickel [black pad]. We posted it as an attachment to the thread. It's a new feature that the folk at SMTnet.com added for our dancing and dining pleasure. Well, maybe not that, but we'll be able to communicate better, anyhow. Coo, eh?

Thanks guys.

Attachments:

reply »

#53322

Able To Post Image | 23 January, 2008

Very cool. Now, how big was that image? It took about 30 seconds to load.

reply »

#53324

Able To Post Image | 23 January, 2008

Took about ten seconds for me, but still, 963kb's in .bmp format. Had you saved in .jpg format, it would have been 43kb.

Either way, sweet feature. Unfortunately if people upload images nearly 1mb in size, I doubt the feature will stick around long. Storage is cheap, but not that cheap.

------ Ben T.

http://bent.gotdns.com/circuitsmart

reply »

#53350

Able To Post Image | 23 January, 2008

Good suggestion. We used a program to convert our bmp to jpg. Much better.

reply »

#53351

Able To Post Image | 24 January, 2008

Cool! Looks like black crack to me though :)

reply »

#53366

Able To Post Image | 25 January, 2008

You could always open the .bmp in Paint, and then do a "Save as..." and choose .jpg as the file type. Everyone has Paint. Unless of course you're using a Mac, but then you'd probably be a graphic designer anyways...

reply »

#53368

Able To Post Image | 25 January, 2008

This is a great tool. Pictures are worth a thousand words - videos is worth a million.

reply »

#53370

Able To Post Image | 25 January, 2008

Fluid Dispense Pump Integration