Versaflow dross buildup

Views: 1888

#53371

Versaflow dross buildup | 25 January, 2008

Hi all, I have an inconsistent situation. Lately, we seem to have excessive dross buildup in the solder pot which inturn causes the pot to overflow. Has anyone had a similar experience? Here are the details: age of machine= 9 years, flux used= Kester 2331-zx, solder= Multicore bar 63/37. Any insight would be appreciated.

Thanks.

Todd.

reply »

#53475

Versaflow dross buildup | 31 January, 2008

Wave too high,pot temp to high set to 245�C. Solder level too low.