I am looking to manufacture a 'custom' SMT carrier from a material which I believe is called Durastone, does anyone know where I can purchase a piece of this raw material, or indeed any other material which may solve this problem.

reply »

PeterB

#5650

SMT / WAVE solder carriers (pallets) | 20 March, 2001

'Durostone' is available in the UK in 2 forms. Conductive and non-conductive. The conductive version is known as type CAS761.

We use:

Rochling Materials Ltd Waterwells Business Park Waterwells Drive Gloucestershire GL2 4AA United Kingdom Tel: 01452 727900 Fax: 01452 728056 e-mail: andy@roechling.co.uk contact: Andy Phillips

You can either buy the material and have the carriers made yourself or ship the design details (or a sample assembly) to them and they will make them for you. Note: there are some special Health and Safety considerations when machining this type of material.

Hope this information is useful,

Pete B

reply »


K

#5655

SMT / WAVE solder carriers (pallets) | 20 March, 2001

Another source to consider is: Garland Services Company Phone = (972) 494-1911

reply »

#5656

SMT / WAVE solder carriers (pallets) | 20 March, 2001

I had pallets made from Stone Mountain Tool, who are using a similar material. http://www.stonemountaintool.com

reply »

MARK COPLAN

#5683

SMT / WAVE solder carriers (pallets) | 21 March, 2001

CALL US AND WE CAN MANUFACTURE YOUR CARRIER FOR YOU! 949-453-1500

reply »

T Gilmore

#5731

SMT / WAVE solder carriers (pallets) | 26 March, 2001

If you go to AGI's website, http://www.autogroup.com, go to products, wave pallets and materials used. You can view durastone propoerties and buy raw material from them.

Let me know if you have any questions,

Todd Gilmore President AGI

reply »

T Gilmore

#5732

SMT / WAVE solder carriers (pallets) | 26 March, 2001

If you go to AGI's website, http://www.autogroup.com, go to products, wave pallets and materials used. You can view durastone propoerties and buy raw material from them.

Let me know if you have any questions,

Todd Gilmore President AGI

reply »

Rob Fischer

#5780

SMT / WAVE solder carriers (pallets) | 28 March, 2001

Try a search engine and look up "+solder+pallet". Any of the major pallet manufacturers can supply this or any other composite materials that you may be looking for. Of course (as I am employed by EMC) I would prefer you choose my site. Try to keep in mind the unrealized internal costs when designing, machining and assembling your pallets. A lot of companies are out there that do it well, here and there, but there are only a few of us that are consistent.

reply »

FPC* - Fluid Pressure Control - Dispensing Pump

SMT Pick and Place