Hi all, Need advice how to fix RJ45 short issue after wave solder m/c .Few actions taken to resolve this issue but the outcome was inclusive which was 1. Modify wave pallet 2. Change conveyor setting from 0.8meter/minute to 0.7 meter/minute 3. Clear solder dross every 4 hours once. 5. Implemented template for post wave touch operator to inspect and touch up

Still found escapee for this short issue at ICT and FVT station. Please shade some light on How to eliminate this issue. Thanks in advance

Regards carmanah

reply »


bga

#55021

RJ45 Connector short issue after wave | 7 June, 2008

You even try out control/cut the connector lead length & turn the wave pallet loading direction?