Tombstone using LF chips | 31 July, 2008

Hi, Im having problem on tombstone, The part is LF chip component 1005, and my solder paste is WS leded. tombstone is not in a deg angle but one side is soldered but the other side is just sitting on the solder. Looks like my solder can not wick up to the terminal.