Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2580
What is this? I thought 63sn 37pb was the norm. What is with... - Sep 09, 2008 by Logannsan
Silver (Ag). It's a typical composition Regards, Vlad ... - Sep 09, 2008 by Vlad
Logannsan, you may want to check into this a little more ... - Sep 09, 2008 by BoardHouse
As far as I know, they rarely do it with Pb-bassed solders. ... - Sep 09, 2008 by Vlad
Actually it's not rare. I use several pastes from various m... - Sep 10, 2008 by Real Chunks
Isn't that the non-eutectic one that provides the pasty phas... - Sep 10, 2008 by Steve Thomas
That is exactly what I said. Rarely belongs to Cu or Ni :-) ... - Sep 10, 2008 by Vlad
The 2 % is Ag.It is added to prevent leaching silver from th... - Sep 11, 2008 by Mark