Hi All,

I was wondering if any of you have any ideas on what is the optimum angle for the conveyor to pass over the waves on a leaded wave machine ?

Any input would be greatly appriciated.

Regards

Darron

reply »

#56682

Leaded Wave Solder Set Up | 25 September, 2008

7 degrees

reply »

#56699

Leaded Wave Solder Set Up | 25 September, 2008

Best is 7 or 6.5D if you cant achieve 7. In fact this is the best angle for Leaded and Lead Free, so watch the Chinese machines as they come in around 5 and cause loads of bridging problems