QFN on UIC's GSM1 | 5 December, 2008

We are running an older GSM1 machine (sw.runs on OS/2) and I would appreciate any hints which vision algorithm to use for best results with QFN and similar parts. One of the ULC's is 2.6mil/pixel.

- Dejan

reply »

#57517

QFN on UIC's GSM1 | 5 December, 2008

I think you can go with PLCC and j lead type. If not go with UIC C type. Both should work Regards, Emil

reply »

#57522

QFN on UIC's GSM1 | 5 December, 2008

I have an 1 year old advantis with flexjet 3 head I tried using the on the head cameras with little luck using the upward looking cameras and putting the part defanition as a QFP using gull-wing leads mesuring the part as is seem to work best thats what universal recamended to me lots of luck

reply »

#57534

QFN on UIC's GSM1 | 8 December, 2008

We run a bunch of .5mm qfn on a GSM1 with a 2.6mil camera, from 16 pad to 100 pad. Works like a charm. We call them a PLCC.