SMT layout for multiple packages | 26 April, 2001

I'm looking for information (links) to pad design and layout spec's for different sized passive SMD's. To be specific, 0603, 0805, 1206 and 3216 sized parts. I'm most interested in finding out about land spacing between two parts. What is accepable/unacceptable? How close can two parts (lands) be situated next to each other without risk of bridging when wave soldered using epoxy deposition on the bottom of the board? ANY help is greatly appreciated.

reply »

#6119

SMT layout for multiple packages | 27 April, 2001

Check out IPC SM-785 Land pattern guidelines for SMT www.ipc.org

Phil