hi,
i am proccess eng solder wave process.I have problem wi...
- May 26, 2009
by
iv40
Is the components on the top or on the bottom of the pcb?
...
- May 26, 2009
by
xinxi
all components ar on the top side...
regards
...
- May 27, 2009
by
iv40
Have you tried profiling the board with temperature label or...
- May 27, 2009
by
xinxi
Please describe the break in the components. Attaching pictu...
- May 27, 2009
by
davef
The problem could be that the preheat temp of the PCB is too...
- May 29, 2009
by
Mark
It would help to see pictures, but I suspect the parts are s...
- May 29, 2009
by
ScottE