BTU -Paragon 150 | 12 November, 2009

Dear All,

I have a problem with the BTU-Paragon 150 10 Zone Reflow Oven. Am not able to lift the HOOD using the buttons on the Main control panel. I have checked the Lift hood switch & Ok. Pls. advice / Suggest.

Thx in advance for all your sincere postings.

With Cheers,

Nagesh

reply »

#60468

BTU -Paragon 150 | 18 November, 2009

Hello I had similar problem on VIP 70A. Try to check auxiliar contact from located into front panel.

Everton - BRAZIL

reply »

#60469

BTU -Paragon 150 | 18 November, 2009

> Dear All, > > I have a problem with the > BTU-Paragon 150 10 Zone Reflow Oven. Am not able > to lift the HOOD using the buttons on the Main > control panel. I have checked the Lift hood > switch & Ok. Pls. advice / Suggest. > > Thx in > advance for all your sincere postings. > > With > Cheers, > > Nagesh

Hello,

I had similar problem on VIP 70A. Try to check auxiliar contacts located into front panel.

Everton - BRAZIL