solder on gold fingers

Views: 4108

#60895

solder on gold fingers | 22 January, 2010

Is there anyway to get solder off gold fingers besides replating them?

reply »

#60897

solder on gold fingers | 22 January, 2010

#60900

solder on gold fingers | 22 January, 2010

My old boss bought some stuff to clean the lead off of gold fingers. At least that is what he thought it did. What it really did was remove the gold fingers. And quite well I might add.

The short answer to your question is no. And if you replate make sure you strip all the metal off first.