Hi,

we have vitronics delta 6622 in your production.Problem with fluxer starting 3 weeks ago.Fluxer moving, but not spraing????I check flux system , and dont find any problems with machine.Clean the spray nozzle with compressed air , but nothing.may be some of you can help me?Flux is cobar 396 VOC free

reply »

#61383

vitronics delta 6622 fluxer | 17 March, 2010

Is it the pressurized system or the pump system you have fitted to the machine? Are you getting an error message 'No flow nozzle 1'? Check the 'ShoRate' gauge at the back of the machine and make sure the ball bearing rises in the glass tube when you are purging. Check all quick fit connectors. Check for blockages by removing the pipes at different points and make sure you have flow. I hope this helps.

reply »

#61388

vitronics delta 6622 fluxer | 18 March, 2010

It is a pressurized system, and , Yes , there are a message "No flow nozzle 1".Our machine have not 'ShoRate' gauge at the back of the machine.There are only 3 gauge for flow on the front side , like watch ???

reply »

#61427

vitronics delta 6622 fluxer | 22 March, 2010

Sorry,I saw 'ShoRate' gauge at the back of the machine.Yes, when fluxer working, the ball moving.But from fluxer head flow only air.