Last July I posted a query about reflowing leaded paste to gold plated boards, I wasn't getting a good reflow. The answer that seemed to work was dwelling the board at reflow for the maximum recommended amount of time. Would anyone have an opinion on this?

Also, I am having trouble finding this query. If I search by name, I only get results where someone used my name in their response. Then under options I clicked show threads for the last 365 days, but it only went back to January 18th. A pre-thanks for any help.

reply »

#62074

Gold finish/ searching threads | 17 June, 2010

> Last July I posted a query about reflowing leaded > paste to gold plated boards, I wasn't getting a > good reflow. The answer that seemed to work was > dwelling the board at reflow for the maximum > recommended amount of time. Would anyone have an > opinion on this? > > Also, I am having trouble > finding this query. If I search by name, I only > get results where someone used my name in their > response. Then under options I clicked show > threads for the last 365 days, but it only went > back to January 18th. A pre-thanks for any help.

I figured out how to find my old query, click advanced search on the left. Still anyones thought on soldering to gold finish would be appreciated. Thanks.

reply »

#62152

Gold finish/ searching threads | 30 June, 2010

You'd don't solder to gold finishes. The gold finish goes in solution in the solder and the solder attaches to the underlying surface, commonly nickel or copper.