Can we apply staking after conformal coating.

Views: 5398

#63037

Can we apply staking after conformal coating. | 2 November, 2010

Dear Team,

Can we apply staking after conformal caoting? If we do this can we expect any future problems. Please clarify our Doubt.

Your reply in this regard is highly appreciated.

Thanks & Regards, Raghuveer S. Medha Servo Drives Pvt Ltd.

reply »

#63109

Can we apply staking after conformal coating. | 11 November, 2010

We don't know, there are lots of different conformal coating materials and staking materials. Not all combinations behave similarly.

Our choice would be to epoxy the component to the board, then conformal coat.

reply »

#63114

Can we apply staking after conformal coating. | 12 November, 2010

thanks for your reply sir,

for conformal coating Humiseal 1B31, what are the preferable staking materials? please suggest us..

reply »

#63182

Can we apply staking after conformal coating. | 24 November, 2010

I would suggest Zymet CN-1703 for staking of the components using this coating material we use it very extensively with Humiseal 1B31, if you would like; I would be happy to coat a couple of your samples for your evaluation.

reply »

#63186

Can we apply staking after conformal coating. | 25 November, 2010

Thanks for your reply sir...

Please tell me, materials you have suggested are reworkable or not...?

reply »

#63216

Can we apply staking after conformal coating. | 30 November, 2010

> Thanks for your reply sir... > > Please tell me, > materials you have suggested are reworkable or > not...?

Yes, The material is reworkable, go you Zymet's website you will find all the information located there.

reply »