solder joint failure analysis | 8 February, 2011

hi, I am a Hardware designer . One of my products is undergoing a Reliability test in which a resistor shows a high value on board from its specified value .However it retains the original value when its cooled under room temperature. The resistor was always subjected to an ambient dry heat temperature of 75 Deg Celcius. The solder joints looks fine and qulifies IPC specs. Can i get some information of 1) Any method to identify the solder quality in terms whether any contamination ,properties changes 2) Any effect of electromigration - the resistor is the series resistor for a pierce crystal configuration

reply »

Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

SMT spare parts - Qinyi Electronics