Is there a simple test available to test for lead content of solder. I don't need to know the specific amount. I just need to know if there is any lead present at all.

reply »

#63774

Testing for Lead Content | 16 February, 2011

Maybe one of those test kits with lead detecting 'swabs'? Changes color when lead is present.

reply »

#63775

Testing for Lead Content | 16 February, 2011

Exactly! Who distributes them?

reply »

#63790

Testing for Lead Content | 18 February, 2011

EIS has them P/N 2515-N LEAD-CHECK SWABS, 8 SWABS, 10BX/CS Manufactured By: ITW TECH SPRAY USD$ 29.53 Per 1 BX I have no affiliation with EIS