I am having issues with Solder balls on Ceramic devices, all...
- Mar 21, 2011
by
N Anderson
Are the solder balls what we would call ' mid chip ' solder ...
- Mar 25, 2011
by
Graham
We have the occasional solder fine but the main issue I have...
- Mar 25, 2011
by
N Anderson
Have you checked your reflow profile? You need top make sure...
- Mar 25, 2011
by
aci
If other solder joints are okay then it is unlikely to be a ...
- Mar 25, 2011
by
Graham
Graham, good idea about reflowing first. I'll try this out.
...
- Mar 28, 2011
by
N Anderson
I would suggest doing an aperture reduction on your stencil ...
- Mar 31, 2011
by
Mark