solder alloy preforms | 18 April, 2011

Hello,

I look for manufacturers of solder preforms.

Found one but seems too expensive and I wonder if are there any more manufacurers of similar product ?

Regardas, AM

Attachments:

reply »

#64179

solder alloy preforms | 19 April, 2011

While you're waiting for others to reply, search the fine SMTnet Archives. For instance, here's a previous thread: http://www.smtnet.com/Forums/index.cfm?fuseaction=view_thread&CFApp=1&Thread_ID=13374&#Message56921

reply »

#64183

solder alloy preforms | 19 April, 2011

Not sure who you've already looked at, but i know Alpha Metals has preforms.

reply »

#64196

solder alloy preforms | 21 April, 2011

Indium Corpo of America is selling preforms..

reply »

#64202

solder alloy preforms | 22 April, 2011

Kester sells preforms.

reply »

#64242

solder alloy preforms | 29 April, 2011

Thank you all for feedback

reply »

#64244

solder alloy preforms | 29 April, 2011

Our company is finishing up a design prototype for an easy to use re-balling fixture. 100% ball attach, and you can re-ball more than one BGA at a time. Initial investment will be in fixture cost, but you will be able to re-ball several chips in around 5 minutes at a cost of $0.006 per solder ball. We will do a press release here on SMTnet in about two weeks with complete details once our final design and testing is complete. We also have a universal re-balling fixture available at: http://www.pcb-repair.com/reballing_kits.htm