Hi
I have seen some of our multilayer PCBs are having del...
- Jun 13, 2011
by
Milroy
Delamination almost always is caused by moisture in the PCB....
- Jun 13, 2011
by
aci
We find it is a bigger issue in the summer when there is mor...
- Jun 13, 2011
by
DeanM
What are your Bake Requirements?
As in temp, duration, etc....
- Jun 13, 2011
by
garyr
Hi Milroy,
One thing to check is the FR4 Laminate being u...
- Jun 16, 2011
by
BoardHouse
What is the correct FR4 for RoHS? This PCB is a 4layer board...
- Jun 20, 2011
by
Milroy
if its a RoHs Assembly they should be using an FR4 material ...
- Jun 22, 2011
by
BoardHouse