Hi, I am facing some problems on my soldering joint. My operators perform the solder and left the assembled PCBs on the WIP rack. After 1 week (Due to shortage of components),the solder joint of the components darken. Is it caused by oxidation? If yes, how can i prevent it. My factory is in a humid and hot country.

thanks for the advice....

reply »

#65528

Dark Solder Joint | 25 November, 2011

This is not what we'd expect. We need more information about process, materials, and distribution of the problem. Also, a picture would be nice.

reply »

#65603

Dark Solder Joint | 7 December, 2011

If this is a water soluble flux, then the discoloring is caused by the still active flux microetching the solder fillets.

Prevention is to wash off all water soluble flux as soon as possible