Can anyone suggest a good underfill compound that is readily... - Feb 21, 2012 by Dennis O'Donnell
Have had good results with Loctite 3536 and Hysol 4527. T... - Feb 21, 2012 by Hegemon
I use Loctite 3567. here's a link to the Data sheet. ... - Feb 24, 2012 by Grant Kim