Hi Guys,
I´m looking for information about processing smt c...
- May 16, 2012
by
FGH
Here's some notes from a Bob Willis presentation
Assembly...
- May 16, 2012
by
davef
Many thanks davef
...
- May 17, 2012
by
FGH
These notes are from ~2005-6. I remember pictures of the pal...
- May 17, 2012
by
davef
Hi,
Since you're looking information about flexible print...
- May 18, 2012
by
msPCB
Ask for board fiducials if you're running arrays. Global fi...
- May 21, 2012
by
SWAG
Polymide is like a sponge and absorbs moisture much faster t...
- May 21, 2012
by
hoss67
If your washing them in-line, heavy silicon mesh works good ...
- May 22, 2012
by
SWAG
There is also a good reference book on flexible circuits fro...
- May 23, 2012
by