Conformal Coating Masking

Sully

#6803

Conformal Coating Masking | 7 June, 2001

Does anyone know of a good masking material for conformal coating? The coating is silicon based. Any help would be greatly appreciated.

Thanks

reply »

Howie

#6933

Conformal Coating Masking | 18 June, 2001

The adhesive type is the problem generally - latex adhesives used are not compatible with the silicone. Humiseal offer silicone compatible tapes & dots although they are quite expensive. I found a 3M product which is compatible with silicone based coatings - it's called "Powder coat masking tape". ( Blue colour - don't have the 3M product number to hand.) This tape is tough to peel off after a thermal cure but is effective. Best advice is to forget the tape masking process and use masking boots if possible - for connectors try the mating connector for the type used. We also use custom machined masks which pay for themselves very quickly when compared to the masking and de-masking time required. For edge masking try using a plastic profile paper binder - you know the type you slide paper into for a report ! It's cheap and cheerful. Regards

reply »

Sully

#6942

Conformal Coating Masking | 18 June, 2001

Thank you very much for your help!

reply »

Boca

#6996

Conformal Coating Masking | 20 June, 2001

I'm interested in the masking boots and covers you mentioned. We have looked at them before, but we use an acrylic conformal coat and clean up with toluene. All of the boot type products we have looked at seem to breakdown in toluene. Do you reuse boots and covers? What are your experiences? Who are your 'boot' suppliers?

Looking forward to your responses.

Boca

reply »

#7004

Conformal Coating Masking | 20 June, 2001

Try: * KINNARNEY RUBBER 450 Main St. P.O.Box 37 Mantua, N.J. 08051 609-468-1320 fax 7438 http://kinnarney.com/ * Dempsey Industries 802 N. 4th St Miamisburg, Ohio 45342 (937)-866-2345 Gary Pascoe * Shercon 10425 Slusher Drive � Santa Fe Springs, CA 90670 (800)228-3218 Fax: (800)955-8988 http://www.shercon.com sales@shercon.com * Harman 360 South St. Rochester, MI 810-651-4477 StockCap St Louis MO 800-827-CAPS (2277) * MOCAP Plastic Products Group 10964 Lin-Valle Drive, St. Louis, MO 63123 800-633-6775 314-845-3100 Fax 487-8855 http://www.mocapinc.thomasregister.com/olc/mocapinc/

reply »