I need help with how long do I need to bake out double sided... - Jul 05, 2012 by cobhambill
Probably they had a problem with a certain product, tried ba... - Jul 05, 2012 by davef
..... that's very strange. If there were any risk of de-lami... - Jul 06, 2012 by jsolloway
All i used to do was blow them with an airline to remove the... - Jul 06, 2012 by TMS
Why cannot reply???? ... - Jul 11, 2012 by Joeion
It is correct to remove moisture in PCB by baking. But I thi... - Jul 11, 2012 by Joeion
Check also the specs / recommendations of your PCB manufactu... - Jul 12, 2012 by Th. Meier
You might try to complete all your soldering within a 72 hou... - Jul 12, 2012 by Hegemon
I appreciate all the feedback. The reason I was asking the q... - Jul 13, 2012 by cobhambill