We have 1/2 dozens 0.031 pcbs that bow after going through t... - Aug 27, 2012 by Reese
Its no my turn to give some advise. My first question would ... - Aug 27, 2012 by cobhambill
Thank you for your reply. > Its no my turn to give som... - Aug 27, 2012 by Reese
I have run 0.031 boards. One of the things you may want to l... - Aug 27, 2012 by cobhambill
We will look at the oven speed. We considered stiffeners bu... - Aug 27, 2012 by Reese
Ran them with stiffners and I worried about moving parts als... - Aug 27, 2012 by cobhambill
We agree with all of the previous comments, and would add th... - Aug 28, 2012 by robgd3
Thank you for your reply. We will try your suggestions and ... - Aug 28, 2012 by Reese